A print that will not stick is almost never a glue problem. It is, in order: a dirty plate, a nozzle sitting too far from the surface, the wrong temperature for the material, and only then a surface or adhesion-aid question. Work them in that order and most adhesion problems end at step one or two.

1. Clean the plate like you mean it

Dish soap, warm water, a clean sponge, full dry, edges-only handling. Skin oil is invisible and decisive. Isopropyl alcohol between prints maintains a clean plate but does not rescue a dirty one; it spreads oil thin rather than removing it. This single step fixes the majority of "suddenly nothing sticks" reports, especially on smooth PEI plates.

2. Set the distance

Lines that stay round and separate, corners that lift as the head moves away, a part that slides when nudged: the nozzle is too far. Lower the Z offset in 0.02 to 0.05 mm steps and print a test patch between steps. Lines should merge into a sheet. Ridges and a scraped, transparent patch mean you have gone too far the other way. The first layer guide describes both failure pictures.

3. Check the temperatures against the material

The slicer profile must match the loaded material: PETG on a PLA profile runs the bed too cool and the part lets go. Confirm the spool, the profile, and the plate type all agree. Bed temperature is a material property from the filament maker's label, not a dial for experimentation.

4. Surface and aids, last

Textured plates grip PLA and PETG differently than smooth ones; PETG on smooth glass or PEI can bond too well and needs a release layer (glue stick as a barrier, not an adhesive). A brim helps small-footprint and tall parts by adding holding area. Adhesive products have their place, on a clean plate, at the right distance: they are the seasoning, not the meal. If a part still will not stick after steps one to three, the honest suspects are a worn plate surface or a warped bed the mesh cannot fully forgive, and the maker's support documentation for your model is the next stop.

Last updated November 28, 2026. Spotted an error? See our corrections policy on the About page.

Questions readers ask

Does glue stick help prints stick?

On the right plate it acts as a release barrier for PETG and a mild adhesion aid for some materials. It cannot compensate for a dirty plate or a wrong Z distance, which is why it is step four on this page, not step one.

Why did prints stick last month and not now?

Plate contamination builds invisibly, and seasonal humidity changes filament and room behaviour. Wash the plate, dry the filament, and recalibrate; that trio resolves most 'suddenly' adhesion stories.

My corners lift but the middle holds. What is that?

That is warping beginning: cooling stress pulling corners up. See the warping page for the cooling, brim, and enclosure logic.