Failed Prints: Work This Order Before Touching Settings
When a print fails and you do not know why, the cause is almost always in the first three items of this list. Work top to bottom, change one thing at a time, and test with a small print after each change. Random setting changes are how a one-cause failure becomes a five-cause mystery.
1. The plate
Dirty plates cause more failures than every setting combined. Wash with dish soap and warm water, dry fully, handle by the edges. If the plate is textured, confirm you are printing on the side and with the profile the maker intends.
2. The first layer
Watch a single-layer test patch. Gaps and round lines mean the nozzle is too far; ridges and ploughing mean too close. Adjust Z offset in 0.02 to 0.05 mm steps. The first layer guide shows what good looks like; the sticking page handles the full adhesion picture.
3. The filament's condition
Popping sounds, steam, foam, sudden stringing: water. Dry the spool or open a fresh one as a test. A known-dry spool is the fastest diagnostic in the hobby because it clears an entire category in one swap. Storage rules are in the storage guide.
4. Extrusion
Clicking, thinning walls, or gaps between lines point to under-extrusion: a partial clog, a slipping extruder gear, a kinked path, or a temperature too low for the material. The nozzle page works this branch. Over-extrusion (blobs, elephant's foot, dimensions fat) is rarer and usually a wrong material profile or flow setting someone changed.
5. Motion
Shifted layers and new noises point to belts, obstructions, and collisions. See the layer shifts page. Check that cables and filament paths cannot snag at full travel in any direction.
6. Settings, last and least
Only now: temperature in 5-degree steps for bonding or stringing questions, supports and orientation for geometry failures, speeds for ringing. Return to the maker's default profile as the control experiment whenever the trail goes cold; a default profile that prints well proves the machine, and isolates your changes as the variable.
Keep a one-line log per failure: model, material, what changed, result. Ten lines of that log will teach you more than a hundred forum threads, because it is data about your machine, your room, and your filament.
Last updated November 28, 2026. Spotted an error? See our corrections policy on the About page.
Questions readers ask
My print failed halfway. Where do I start?
At the top of this page: plate, first layer evidence (the bottom of the failed part tells the story), filament condition, then extrusion and motion. The height at which it failed and the state of the part narrow the branch quickly.
Should I reprint the same file to test?
No: print something small and known. A test patch or a 20 minute object isolates the fix. Reprinting the failed six-hour model as the test is how weekends disappear.
How do I know if it is the machine or me?
Run the maker's included test file on a washed plate with fresh filament. If it prints cleanly, the machine is fine and the variable is your file, settings, or material. That one experiment answers the question definitively.